Influência da madeira na branqueabilidade e estabilidade de alvura de polpas kraft de eucalipto

Mostrar registro simples

dc.contributor.advisor Colodette, Jorge Luiz pt_BR
dc.contributor.author Oliveira, Romildo Lopes de pt_BR
dc.contributor.other Universidade Federal de Viçosa pt_BR
dc.date 2007-12-03 00:00:00.0 pt_BR
dc.date.accessioned 2013-01-22T10:30:39Z
dc.date.available 2013-01-22T10:30:39Z
dc.date.issued 2004 pt_BR
dc.identifier.citation Oliveira, Romildo Lopes de. Influência da madeira na branqueabilidade e estabilidade de alvura de polpas kraft de eucalipto. Viçosa, MG : UFV, 2004. 87 f. : il. (Dissertação - Mestrado em Ciência Florestal) - Universidade Federal de Viçosa. Orientador: Jorge Luiz Colodette. T 634.986117 o48i 2004 pt_BR
dc.identifier.other 118502 pt_BR
dc.identifier.uri http://www.bibliotecaflorestal.ufv.br/handle/123456789/2435
dc.description Dissertação de mestrado defendida na Universidade Federal de Viçosa pt_BR
dc.description.abstract O objetivo deste estudo foi avaliar a influência da madeira, utilizando diferentes clones de eucalipto, na branqueabilidade e estabilidade de alvura de polpas produzidas pelo processo kraft. Foram avaliadas amostras de polpas provenientes de 26 clones de eucalipto de número kappa 16,0 a 17,5. As amostras foram submetidas à deslignificação com oxigênio (pré-O2), eslignificação com dióxido de cloro seguido de extração alcalina simples (DE) e branqueamento ECF (isento de cloro elementar) completo, com as seqüências ODEDD e ODEDP, sendo o desempenho desses processos avaliados pela eficiência, pela seletividade, pelo ganho de alvura e pela estabilidade de alvura (no caso da seqüência completa). O impacto da densidade básica da madeira (398,0 a 558,0 kg/m3), do consumo de álcali efetivo do cozimento (14,1 a 18,0%, como NaOH) e do rendimento depurado de polpa (51,2 a 54,5%) no desempenho dos processos de branqueamento foi também utilizado na interpretação dos resultados. Foi verificado que o tipo de madeira tem influência significativa no desempenho da pré-O2, tratamento DE e do branqueamento completo da polpa. A eficiência, a seletividade e o ganho de alvura da pré-O2, para as 26 amostras, variaram de 28,6 a 40,8%, 0,1 a 0,7 Ud. kappa/Ud. visc., e 15,5 a 31,3% ISO, respectivamente. Para o tratamento DE, as variações foram de 56,3 a 74,1, 0,8 a 3,6 e 33,4 a 41,3, respectivamente. No branqueamento completo pela seqüência ODEDD, a branqueabilidade, seletividade e estabilidade de alvura das polpas variaram de 0,33 a 0,38 Ud. kappa removidas/kg de cloro ativo, 0,3 a 1,3 Ud. kappa/Ud. visc., e 1,9 a 3,2 % ISO, respectivamente. Já no branqueamento pela seqüência ODEDP, a branqueabilidade, seletividade e estabilidade de alvura das polpas variaram de 0,30 a 0,39, 0,3 a 1,0 e 1,1 a 1,4, respectivamente. O ganho de alvura e a eficiência de deslignificação das polpas no tratamento DE foram afetados negativa e significativamente, a 5% de significância, pela demanda de álcali efetivo do cozimento. A seletividade da pré-O2 e do tratamento DE foi afetada, positiva e significativamente, a 5% significância, pela densidade básica da madeira. A eficiência de deslignificação no tratamento DE se correlacionou, positiva e significativamente, com o rendimento depurado de polpa. A demanda de álcali efetivo e a densidade básica da madeira se correlacionaram, positiva e significativamente, com as seletividades dos branqueamentos completos com as seqüências ODEDD e ODEDP. O rendimento depurado se correlacionou, negativa e significativamente, com a seletividade do branqueamento pela seqüência ODEDD, a 5% de significância. Polpas branqueadas pela seqüência ODEDP apresentaram maior estabilidade de alvura que as branqueadas pela seqüência ODEDD. A estabilidade de alvura das polpas é influenciada pelos seus conteúdos de grupos carboxilas e carbonilas e, também, pelo residual oxidável (número de permanganato). pt_BR
dc.description.abstract The objective of this study was to evaluate the influence of the wood, from different eucalyptus clones, an bleachability and brightness stability kraft pulps. kraft pulps from 26 different eucalyptus wood clones were evaluated. The samples of 16.0 - 17.5 kappa number were delignification with oxygen (Pre-O2) and chlorine dioxide (DE treatment) and fully bleaching with the ODEDD and ODEDP sequences. There processes were compared based an efficiency, selectivity, brightness gain an brightness stability (fully bleached pulps only). Also evaluated was the impact of wood density (398.0 - 558.0 kg/m3), effective alkali consumption (14.1 - 18.0% as NaOH) and pulp yield (51.2 - 54.5%) on the performance of such processes. It was concluded that wood type significantly affects the performance of Pre-O2, DE treatment and full pulp bleaching with ODEDD and ODEDP sequences. The values of efficiency, selectivity and brightness gain for the Pre-O2 of the 26 samples varied in the range of 28.6 - 40.8%, 0.1 - 0.7 Ud. Kappa/Ud. viscosity and 15.5 - 31.3% ISO, respectively. For DE treatment the varieties was in the range of 56.3 - 74.1%, 0.8 - 3.6 Ud. kappa/Ud. viscosity and 33.4 - 41.3% ISO, respectively. In the full bleaching with the sequence ODEDD, the values of bleachability, selectivity and brightness reversion varied in the range of 0.33 - 0.38 Ud. kappa/kg Cl2 active, 0.3 - 1.3 Ud. kappa/Ud. viscosity and 1.9 - 3.2% ISO, respectively. For the sequence ODEDP these values varied in the range of 0.3 - 0.39, 0.3 - 1.0 and 1.1 - 1.4, respectively. The delignification efficiency and brightness gain in the DE treatment were significantly, affected by pulping effective alkali. The selectivity of pré-O2 and DE treatment were significantly and positively affected by wood basic density. The delignification efficiency of DE treatment was significantly and positively affected by pulping yield. The selectivity of he full bleaching with the sequences ODEDD and ODEDP was significantly and positively by wood density and pulping effective alkali. The selectivity of ODEDP bleaching correlated significantly and negatively with pulping yield. The was significantly effect of wood type an pulp brightness stability, but no significant correlation was seen between this parameter and wood density, pulping effective alkali and pulping yield. Pulps bleached with the ODEDP sequence showed be the brightness stability them those bleached with the ODEDD sequence. Pulp brightness stability is significantly affected by them contents of carboxyl, carbonyl and oxidizable rendnates (measured by KMnO4 number). en
dc.description.sponsorship Universidade Federal de Viçosa pt_BR
dc.format.mimetype application/pdf pt_BR
dc.language.iso pt_BR pt_BR
dc.publisher Universidade Federal de Viçosa pt_BR
dc.subject Polpa de madeira; Branqueamento; Polpação alcalina por sulfato; Madeira; Qualidade pt_BR
dc.title Influência da madeira na branqueabilidade e estabilidade de alvura de polpas kraft de eucalipto pt_BR
dc.title [Influence of the wood in bleachability and of brightness stability of kraft pulp of eucalyptus] en
dc.title.alternative [Influence of the wood in bleachability and of brightness stability of kraft pulp of eucalyptus] en
dc.type Dissertação pt_BR

Arquivos deste item

Arquivos Tamanho Formato Visualização Descrição
Dissertaçao_Romildo-Lopes-de-Oliveira.pdf 389.2Kb application/pdf Visualizar/Abrir ou Pre-visualizar Dissertação

Este item aparece na(s) seguinte(s) coleção(s)

Mostrar registro simples

Buscar em toda a Biblioteca


Sobre a Biblioteca Florestal

Navegar

Minha conta